+91 8866188126 [email protected]

PCB assembly guide

BGA, QFN and fine-pitch assembly: process, X-ray and rework

Ball grid arrays, land grid arrays, QFNs and tiny 0201 passives make compact, powerful products possible — but their solder joints are either hidden under the package or very small. This guide explains, in general terms, what has to go right at every step, how hidden joints are checked, what rework can and cannot do, and how these parts are handled when you order assembly from Microplacer.

Get an instant quote

Why hidden-joint and fine-pitch parts need extra process control

With a gull-wing SOIC you can see every joint and touch it with an iron. With area-array and bottom-terminated packages the joints are under the body, and with very small chips the solder volume is tiny. Small process variations that a large part tolerates become defects.

Package familyWhere the joints areMain assembly riskCan joints be seen optically?
BGA (ball grid array)Solder balls in a grid under the bodyOpens, bridges, head-in-pillow, voids, warpageOnly the outer row, partially
LGA (land grid array)Flat pads under the body, no ballsVery low stand-off, sensitive to paste volume and flatnessNo
QFN / DFNPads on the underside edge plus a large exposed thermal padThermal-pad voids, part floating or tilting, weak side filletsSide fillet only, if the lead ends are wettable
Fine-pitch QFP / SSOP (about 0.5 mm pitch and below)Visible gull-wing leadsBridging between leads, lifted leads from coplanarity issuesYes, with magnification
0201 (and smaller) chipsTwo tiny end terminationsTombstoning, missing parts, skew, insufficient solderYes, with magnification

Less margin everywhere

Paste volume, placement offset, board flatness and the reflow profile all have to sit inside a narrower window. One weak step is often enough to cause a defect.

Harder to inspect

Automated optical inspection sees what is on the surface. Joints under a body need X-ray, and some faults are hard to detect even then.

Harder to fix

A bridge on a QFP can be wicked with an iron. A bridge under a BGA means removing the whole package, cleaning the site and fitting a new or reballed part.

Why our instant PCBA price sends BGA, LGA and 0201 parts to engineering review

Our instant assembly price is built from the solder pads on your board and the quantity. That works well for standard SMD and through-hole parts, where cost follows pad count closely. Hidden-joint and very small parts add work that pad count alone does not capture.

  1. 1

    You upload your files

    The online quote reads your solder pads and gives an instant assembly price for standard parts. Components are quoted separately from your BOM. See how the assembly quote works.
  2. 2

    BGA, LGA or 0201 parts are detected

    Instead of guessing, these boards go to engineering review. An engineer looks at the packages, pad design, stencil needs and inspection requirements before a price is confirmed.
  3. 3

    Engineers check the design before production

    Our engineers check files before production. Notes you add to your files (for example a required inspection or a moisture-sensitive part) are read and compared with the options we can offer.
  4. 4

    You receive a confirmed quote

    Once the review is done you get a price that reflects the real process for your board, rather than an instant figure that might change later.

Ordering basics that still apply

PCBA is built in panels. Stencils are free for 5 to 50 boards, and from 55 boards a shared stencil is used. The minimum order is 5 PCBs, and payment is made at order time by online payment or bank transfer.

Paste deposit on small pads: stencil thickness, aperture reduction and area ratio

General guidance — the right values depend on the parts on the whole board, the paste type and the assembler’s process. IPC-7525 is the usual reference for stencil design.

Area ratio decides release

Paste only leaves the stencil cleanly if the aperture walls do not hold on to it. A common check is the area ratio: aperture opening area divided by aperture wall area. For a round or square aperture this simplifies to opening width ÷ (4 × stencil thickness). A common rule of thumb is to keep it at about 0.66 or higher; below that, release becomes unreliable.

One stencil, many parts

A single stencil thickness has to suit every part on that side. Large connectors want more paste; 0201s and 0.4 mm-pitch BGAs want less. Fine-pitch boards often settle on a thinner foil and use larger apertures or step areas for the parts that need extra volume.
Feature (typical)Common stencil thickness rangeCommon aperture approach
Standard SMD, 0603/0805, SOICabout 0.12–0.15 mmClose to 1:1 with the pad, small reductions to limit bridging
0.5 mm-pitch QFP / QFN leadsabout 0.10–0.13 mmWidth slightly reduced to leave a gap between deposits
0.8–1.0 mm-pitch BGAabout 0.10–0.13 mmRound or square aperture close to the pad size
0.4–0.5 mm-pitch BGA / CSPabout 0.08–0.10 mmSquare with rounded corners helps release; check area ratio
0201 chipsabout 0.08–0.10 mmReduced or shaped apertures to limit tombstoning and balling
QFN exposed thermal padSame foil as the restSplit into a window-pane pattern, often around 50–80 % coverage

Worked example

A 0.25 mm square aperture in a 0.10 mm foil gives 0.25 ÷ (4 × 0.10) = 0.625 — just below the common 0.66 guideline. The same aperture in a 0.08 mm foil gives about 0.78, which normally releases well. This is why boards with 0.4 mm-pitch parts often need a thinner stencil.

Placement accuracy, board flatness and why a flat surface finish helps

Fine-pitch parts are placed by machine using fiducials and the package outline or ball pattern. During reflow, surface tension pulls many parts toward the pads — but only if the paste, pads and board are in good shape.

Fiducials

Global fiducials on the panel and local fiducials near large fine-pitch parts let the machine correct for small stretch and offset. A clear, mask-free area around each fiducial makes them easy to recognise.

Flat pads

Domed HASL pads can lift one side of a small part or leave uneven paste prints. A flat finish such as ENIG (or OSP if boards are assembled soon) gives an even surface. See the surface finish guide.

Flat boards

Bow and twist lift the board away from the stencil and change the gap under a large BGA. Balanced copper on each layer, a symmetrical stack-up and a suitable thickness all help.
ChoiceEffect on fine-pitch assembly
ENIG finishFlat, solderable pads with a long shelf life — a common choice for BGA, LGA and QFN boards
OSP finishAlso flat and economical, but plan assembly soon after delivery and keep reflow passes close together
HASL / lead-free HASLUneven pad surface; fine for larger parts, less suitable for fine pitch and area arrays
Solder-mask-defined vs copper-defined padsCopper-defined (non-solder-mask-defined) pads are a common default for BGAs; follow the part maker’s land pattern and IPC-7351 guidance

Reflow for large packages: soak, peak temperature, warpage and head-in-pillow

A reflow profile is the temperature-over-time path the board follows through the oven. Large BGAs, heavy copper planes and small passives on the same board heat at different rates, so the profile is a compromise.

  1. 1

    Preheat and soak

    The board warms gradually so the flux activates and large and small parts move closer to the same temperature. Too fast a ramp can cause spattering and thermal stress.
  2. 2

    Time above liquidus

    All joints, including the balls in the centre of a large BGA, must be fully molten for long enough to wet and collapse. Typical lead-free profiles keep joints above liquidus for roughly 45–90 seconds, depending on the paste.
  3. 3

    Peak temperature

    Peak must be high enough to reflow the coolest joint but stay inside the limits given for each component. As general guidance, lead-free SAC alloys such as SAC305 melt at roughly 217–220 °C and are commonly peaked around 235–250 °C, while eutectic tin-lead melts at 183 °C and is commonly peaked around 205–225 °C. J-STD-020 defines the package peak-temperature classifications that part makers publish.
  4. 4

    Controlled cooling

    A steady cool-down gives a sound joint structure and limits stress between the package and the board.

Warpage

Packages and boards both bend slightly as they heat. If the corners of a BGA lift while the board sags, some balls lose contact with the paste at the critical moment.

Head-in-pillow

The ball and the paste both melt but do not merge, because they were apart while molten and the surfaces oxidised. After cooling the ball rests in the paste like a head on a pillow. It may pass an electrical test and fail later, and it can be hard to see even on X-ray.

Moisture-sensitive parts

Many plastic packages absorb moisture from the air. Heated quickly in reflow, that moisture can crack the package or delaminate it internally. Parts are handled according to their moisture sensitivity level (MSL), with floor-life limits and baking where needed, following J-STD-033. Tell us if parts you supply have been out of their sealed bags. See MSL, ESD and component handling.

Voids under BGAs and thermal pads: causes and how window-pane apertures reduce them

A void is a gas pocket trapped in a solder joint. Some voiding is normal; large voids reduce strength and, under a thermal pad, raise the operating temperature of the part.

Common causeWhy it creates voidsTypical mitigation
Large continuous paste depositFlux gases cannot escape from the middle of a big areaWindow-pane (segmented) apertures leave escape channels
Open vias in the thermal padSolder drains into the hole and air rises out of itFilled and capped vias, or tented/plugged vias where suitable
Via-in-pad under a BGA ballThe open hole traps gas and steals solder from the ballEpoxy or copper-paste filled and capped vias
Profile and paste choiceShort soak or high-voiding flux chemistryAdjusted soak, a lower-voiding paste

Window-pane apertures

Instead of one big opening over a QFN thermal pad, the stencil has a grid of smaller openings with webs between them. This reduces the paste volume (lowering the risk of the part floating) and gives gas a path out.

How much voiding is acceptable?

Acceptance criteria are product-specific. IPC-A-610 and IPC-7095 give general guidance for BGA voids; thermal-pad limits usually come from the part maker or your own thermal analysis. State any limit you need when ordering.

Checking hidden joints with X-ray: what it shows and what it cannot prove

X-ray passes through the package and board; solder absorbs more of it than plastic, copper traces or laminate, so joints appear as dark shapes.

X-ray usually shows wellX-ray may miss or cannot prove
Bridges between balls or under QFN padsHead-in-pillow, where the ball and paste are touching but not fused
Missing or misaligned ballsCold or poorly wetted joints that still have a normal shape
Void size and positionCracks in a joint that are thin compared with the beam path
Ball size differences that suggest an open or insufficient jointLong-term reliability of a joint

2D X-ray

A top-down view. Fast and good for bridges, voids and alignment, but features on both sides of the board can overlap.

Angled / oblique views

Tilting the view shows ball shape and helps separate a joint from parts on the other side.

Combine with other tests

Electrical and functional tests catch faults X-ray cannot see. See testing and inspection.

Rework and reballing: when a BGA can be replaced, and the limits

Hidden-joint parts can often be reworked, but each removal heats the board, the part and its neighbours again. Rework is a repair, not a substitute for getting the first build right.

  1. 1

    Pre-bake if needed

    Boards and parts that may have absorbed moisture are baked first so the reheat does not damage them.
  2. 2

    Remove the part

    A rework station heats the package from above with a focused nozzle while heating the board from below, until all joints melt and the part can be lifted.
  3. 3

    Prepare the site

    Old solder is removed from the pads without lifting them or damaging the mask, then the site is cleaned.
  4. 4

    Reball or replace

    A new part is used, or a removed BGA is reballed by applying new solder balls through a fixture and reflowing them.
  5. 5

    Refit and verify

    Fresh flux or paste is applied, the part is aligned and reflowed with a local profile, then checked with X-ray and electrical testing.

Limits of BGA rework

Pads can lift and laminate can blister after repeated heating; a common practice is to limit the number of rework cycles per site. Underfilled parts are much harder to remove. Neighbouring parts within a few millimetres may reflow too, and tall parts can block the nozzle. Keeping some clearance around large BGAs makes rework far easier. See repair and rework.

Designer checklist

Use this before you send files. For general layout rules see design for assembly; for via-in-pad fanout see vias and special holes.

CheckWhy it matters
Use the part maker’s recommended land pattern (IPC-7351 style)Pad size and mask definition set paste volume and joint shape
Choose a flat finish (ENIG, or OSP for quick assembly)Even paste print and good coplanarity under area arrays
Fill and cap any via inside a padOpen holes steal solder and cause voids; our online calculator offers epoxy filled & capped and copper paste filled & capped via options
Segment thermal pads in the paste layer, or ask about it in your notesReduces voids and part floating
Add local fiducials near large fine-pitch partsBetter placement correction
Keep clearance around BGAsRoom for a rework nozzle and for X-ray views
Balance copper and keep the stack-up symmetricalLess warpage during reflow
Mark pin 1 / A1 clearly on silkscreen and assembly drawingPrevents rotated placement

Board options to pick for BGA designs

In our online calculator, choose ENIG as the finish and select the via covering that matches your design — tented for standard vias, or epoxy filled & capped / copper paste filled & capped for via-in-pad. Fine-via options depend on layer count and finish; see PCB capabilities for current limits.

What to send us and what to specify when ordering

Complete files make the engineering review faster. See design files for formats.

Gerbers with paste layers

Include top and bottom paste layers. If you have already designed window-pane or reduced apertures, say so in your notes so they are kept.

BOM with exact part numbers

Full manufacturer part numbers and package codes, so we quote the right parts. Components are quoted from your BOM; browse electronic components.

Pick-and-place / centroid file

Rotation and pin-1 orientation for every part, especially BGAs and QFNs.

Assembly drawing and notes

Polarity, A1 markers, any part that must not be fitted, and parts that need special handling.

Inspection and acceptance requirements

If you need X-ray of specific parts, a void limit, or an IPC-A-610 class, write it in your notes. Our engineers read these notes and compare them with our options.

Customer-supplied parts

Tell us the moisture sensitivity level and whether the bags have been opened, and send parts in their original packing where possible.

Frequently asked questions

Boards with BGA, LGA or 0201 parts go to engineering review instead of the instant price, so an engineer can check pads, stencil and inspection needs before confirming the cost.

QFNs have visible side terminations and are usually less demanding than BGAs, but the thermal pad still needs a good paste design. Our engineers check files before production either way. See the assembly quote FAQ.

A flat finish. ENIG is a common choice because it is flat and stores well; OSP is also flat if you assemble soon. See the surface finish guide.

Only if the vias are inside the pads (via-in-pad). Then they should be filled and capped so solder is not drawn into the hole. Dog-bone fanout with tented vias between pads normally does not need filling.

No. X-ray is very good at finding bridges, missing balls and voids, but defects like head-in-pillow or poor wetting can look normal. It is best combined with electrical and functional testing.

Often yes, by removing it, preparing the site and fitting a new or reballed part. Each rework cycle stresses the pads and laminate, so the number of attempts is limited and success depends on the layout around the part.

Stencils are free for 5 to 50 boards; from 55 boards a shared stencil is used. Special stencil needs for fine-pitch parts are discussed during the engineering review.

Related guides

Still have a question?

Send us your files or call us — our engineers will help you choose the right options for your boards and assembly.

Streamline your innovation with seamless PCB ordering.